Bột phun hvof của hãng tafa-usa
Name |
Nominal Chemistry |
Powder Name |
Flow Density |
Size |
Approved Specs |
Similar Powders |
Spray Process |
Application Data |
Chromium Carbide Based Powders |
||||||||
Cr3C2 Sintered |
Cr3C2 99.0 min |
CRC-105 |
neg. 2.3 g/cm3 |
-325 mesh/+5 µm -45 µm/+5 µm |
PWA 1304 |
70F-NS |
|
Usually blended with a metal for spraying Hard and wear resistant Useful up to 1600°F (871°C) |
CRC-107 |
30 sec 2.4 g/cm3 |
-140/+325 mesh -106 µm/+45 µm |
PWA 1306 |
70C-NS |
|
|||
Cr3C2-7NiCr Blended |
Ni 5.5 C 12.5 Cr Rem |
CRC-184 |
neg. 2.4 g/cm3 |
-325 mesh/+10 µm -45 µm/+10 µm |
PWA 1364 |
82VF-NS 3005 |
|
Similar to 75/25 Cr3C2-NiCr, but higher Cr3C2 increases hardness Good hot gas and corrosion resistance Hard and wear resistant Useful up to 1600°F (871°C) |
Cr3C2-25NiCr Blended |
Ni 20.0 C 10.0 Cr Rem |
CRC-106 |
neg. 2.5 g/cm3 |
-325 mesh/+5 µm -45 µm/+5 µm |
AMS 7875 B50TF137 CLA MSRR 9507/17 M3965 PM 819-05 EMS 52432 II |
81 VF-NS 3004 |
|
Excellent for high temperature cavitation, abrasion and sliding wear Good hot gas and corrosion resistanceHard and wear resistantUseful up to 1600°F (871°C) |
CRC-108 |
30 sec 2.5 g/cm3 |
-140 mesh/+20 µm -106 µm/+20 µm |
B50TF137 CLB PWA 1307 MSRR 9507/2 EMS 52432 II |
81 NS |
|
|||
Cr3C2-25NiCr Agglomerated and Sintered |
Ni 20.0 C 10.0 Cr Rem |
1375VM |
32 sec 2.3 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
Amdry® 5260 |
|
Excellent for high temperature cavitation, abrasion and sliding wear Good hot gas and corrosion resistance Very dense and hard coatings Useful up to 1600°F (871°C) |
1375VF |
neg. 2.3 g/cm3 |
-400 mesh/+10 µm -38 µm/+10 µm |
|
|
|
|||
Cr3C2-25NiCr Densified |
Ni 20.0 C 10.0 Cr Rem |
1376T |
19 sec 3.1 g/cm3 |
-270 mesh/+20 µm -53 µm/+20 µm |
|
|
|
Excellent for high temperature cavitation, abrasion and sliding wear Good hot gas and corrosion resistance Exceptional flow Useful up to 1600°F (871°C) |
CrC-30NiCr Activated |
Ni 8.0 C 4.0 Cr Rem |
CRC-410 |
17 sec 3.9 g/cm3 |
-270 mesh/+15 µm -53 µm/+15 µm |
|
|
|
Improved DE and stress properties over traditional blended CrC-NiCr Excellent for high temperature cavitation, abrasion and sliding wear Good hot gas and corrosion resistance Useful up to 1600°F (871°C) |
CRC-410-1 |
19 sec 3.7 g/cm3 |
-325 mesh/+10 µm -325 µm/+10 µm |
|
|
|
|||
CRC-410-2 |
17 sec 3.9 g/cm3 |
-140/+325 mesh -106 µm/+45 µm |
|
|
|
|||
CrC-65NiCr Activated |
Ni 10.0 C 2.0 Cr Rem |
CRC-415 |
18 sec 4.0 g/cm3 |
-270 mesh/+15 µm -53 µm/+15 µm |
|
|
|
Similar to CRC-410, with improved ductility, toughness and corrosion resistance but with lower hardness |
CRC-415-1 |
20 sec 3.8 g/cm3 |
-325 mesh/+10 µm -325 µm/+10 µm |
|
|
|
|||
CRC-415-2 |
17 sec 3.9 g/cm3 |
-140/+325 mesh -106 µm/+45 µm |
|
|
|
|||
CrC-40NiCr Activated |
Ni 22.0 C 3.4 Cr Rem |
CRC-425 |
17 sec 4.0 g/cm3 |
-270 mesh/+15 µm -53 µm/+15 µm |
|
|
|
Similar to CRC-410, but with improved ductility and better toughness with slightly lower hardness |
CRC-425-1 |
20 sec 3.9 g/cm3 |
-325 mesh/+10 µm -325 µm/+10 µm |
|
|
|
|||
CRC-425-2 |
17 sec 3.8 g/cm3 |
-140/+325 mesh -106 µm/+45 µm |
|
|
|
|||
Name |
Nominal Chemistry |
Powder Name |
Flow Density |
Size |
Approved Specs |
Similar Powders |
Spray Process |
Application Data |
Tungsten Carbide Based Powders |
||||||||
WC-8Co Sintered |
Co 8.0 C 5.2 min W Rem |
AI-1071 |
20 sec 5.0 g/cm3 |
-200/+325 mesh -75 µm/+45 µm |
|
|
|
Commercial grade of WC-Co Dense, hard wear resistant coating Useful up to 900°F (482°C) |
AI-1171 |
neg. 5.0 g/cm3 |
-325/+15 µm -45 µm/+15 µm |
|
|
|
|||
WC-12Co Cast |
Co 11.0 C 3.9 W Rem |
WC-104 |
12 sec 6.1 g/cm3 |
-200/+325 mesh -75 µm/+45 µm |
PWA 1302 EMS 57745 |
71NS Amdry® 302 |
|
Excellent low temperature wear properties Dense, hard coating with marginal oxidation and corrosion resistance Useful up to 900°F (482°C) |
WC-106 |
neg. 5.9 g/cm3 |
-325 mesh/+5 µm -45 µm/+5 µm |
PWA 1379-2 AMS 7879 BMS 10-67-1 |
71VF-NS Amdry® 301 |
|
|||
WC-12Co Sintered |
Co 11.0 C 4.0 W Rem |
1320Q |
neg. 5.0 g/cm3 |
-325 mesh/+5 µm -45 µm/+5 µm |
|
71 VF-NS Amdry® 301 |
|
Excellent low temperature wear properties Dense, hard coating with marginal oxidation and corrosion resistance Useful up to 900°F (482°C) |
WC-12Co Sintered |
Co 12.0 C 5.3 W Rem |
WC-114 |
16 sec 4.9 g/cm3 |
-325 mesh/+10 µm -45 µm/+10 µm |
AMS 7880 B50TF27 CLA/B PM 819-25 |
72F-NS |
|
Excellent low temperature wear properties Dense, hard coating with marginal oxidation and corro- sion resistance Useful up to 900°F (482°C) |
WC-489-1 |
16 sec 4.9 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
|
|
|||
WC-12Co Agglomerated and Sintered |
Co 12.0 C 5.4 W Rem |
1342VM |
20 sec 4.4 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
SM 5812 |
|
Similar properties as other WC-12Co Densified structure with fine carbide dispersion promotes finer microstructure, better DE and denser, smoother coatings Excellent flowability |
1342VF |
18 sec 4.3 g/cm3 |
-400 mesh/+10 µm -38 µm/+10 µm |
|
2004 |
|
|||
WC-17Co Agglomerated and Sintered |
Co 17.0 C 5.3 W Rem |
1343VM |
20 sec 4.3 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
Amdry® 9831 |
|
Higher Co levels provides better toughness, impact strength and ductility than WC-12Co Densified structure promotes superior coating density and powder flow Excellent flowability |
1343V |
18 sec 4.4 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
PWA 36331-1 |
73F 73F-NS-2 |
|
|||
1343VF |
neg. 4.2 g/cm3 |
-400 mesh/+10 µm -38 µm/+10 µm |
|
2005NS |
|
|||
WC-10Ni Agglomerated and Sintered |
Ni 10.5 C 3.6 W Rem |
1310VM |
20 sec 4.4 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
|
|
Better corrosion protection than WC-Co Excellent low temperature wear properties up to 900°F (482°C) Superior deposition efficiency |
1310VF |
19 sec 4.5 g/cm3 |
-400 mesh/+10 µm -38 µm/+10 µm |
|
|
|
|||
WC-Co-Cr Sintered |
Co 10.0 Cr 4.0 C 5.3 W Rem |
WC-113 |
neg 4.5 g/cm3 |
-325 mesh/+5 µm -45 µm/+5 µm |
|
|
|
Improved oxidation and corrosion protection over WC-Co and WC-Ni Excellent low temperature wear properties Useful up to 900°F (482°C) |
WC-436-1 |
18 sec 4.5 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
|
|
|||
WC-Co-Cr Agglomerated and Sintered |
Co 9.5 C 5.2 W Rem |
1350VM |
19 sec 4.5 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
|
|
Similar properties as other WC-Co-Cr Densified structure with fine carbide dispersion promotes finer microstructure, better DE and denser, smoother coatings Excellent flowability |
1350VF |
18 sec 4.6 g/cm3 |
-400 mesh/+10 µm -38 µm/+10 µm |
|
Amdry® 5843 |
|
|||
WC-CrC-Ni Sintered |
Cr 20.0 Ni 6.0 C 5.8 W Rem |
WC-496 |
21 sec 3.2 g/cm3 |
-325 mesh/+15 µm -45 µm/+15 µm |
|
|
|
Superior oxidation and corrosion properties than other tungsten carbide based material Better chemical resistance that other tungsten carbide based materials Useful up to 1400°F (760°C) |
WC-CrC-Ni Agglomerated and Sintered |
Cr 21.0 Ni 6.0 C 5.0 W Rem |
1356VM |
20 sec 4.4 g/cm3 |
-325 mesh /+15 µm -45 µm/+15 µm |
|
|
|
Similar properties as other WC-CrC-Ni Densified structure with fine carbide dispersion promotes finer microstructure, better DE and denser, smoother coatings Excellent flowability |
WC-12Co +50Ni SF Blended |
Ni 35.0 Cr 8.0 Co 6.0 C 3.0 W Rem |
1334F |
22 sec 4.3 g/cm3 |
-270 mesh /+15 µm -53 µm/+15 µm |
|
|
|
Excellent combination of abrasion resistance and toughness Economical solution to severe wear applications |